Slag inclusion is the welding defect caused by ___________________.

This question was previously asked in
RRB JE ME 22 Apr 2025 Shift 2 CBT 2 Official Paper
View all RRB JE Papers >
  1. gas being trapped, due to moisture
  2. insufficient cleaning and preparation of the base metal before welding commences
  3. contamination of either the filler or parent metals
  4. incorrect edge penetration

Answer (Detailed Solution Below)

Option 2 : insufficient cleaning and preparation of the base metal before welding commences
Free
General Science for All Railway Exams Mock Test
2.2 Lakh Users
20 Questions 20 Marks 15 Mins

Detailed Solution

Download Solution PDF

Explanation:

Slag inclusion: 

  • Slag Inclusions are a common welding defect that occurs when slag a welding byproduct gets stuck inside the weldment. This is an unfavorable condition that creates performance issues down the line. In most cases it is a result of bad welding techniques or improper selection of components and parameters.
  • These slag inclusions frequently appear at the edges of a weld if the correct welding procedure is not used.

  • The molten slag being lighter than the weld metal rises to the surface of the liquid pool rapidly forming a blanket that covers the metal. Furthermore the slag solidifies at a lower temperature than the metal. Thus when an edge is not completely filled with metal and has a drooping contour the slag blanket slips around this contour and settles in the corner. When the metal solidifies more slag will settle in the edge to form a tightly adhering inclusion.

Main Causes Of Slag Inclusions: 

  • Type Of Flux Used
  • Welding Parameters
  • Poor Welding Technique
  • Bad Practices
Latest RRB JE Updates

Last updated on Jul 2, 2025

-> The RRB JE CBT 2 Result 2025 has been released for 9 RRBs Zones (Ahmedabad, Bengaluru, Jammu-Srinagar, Kolkata, Malda, Mumbai, Ranchi, Secunderabad, and Thiruvananthapuram).

-> RRB JE CBT 2 Scorecard 2025 has been released along with cut off Marks.

-> RRB JE CBT 2 answer key 2025 for June 4 exam has been released at the official website.

-> Check Your Marks via RRB JE CBT 2 Rank Calculator 2025

-> RRB JE CBT 2 admit card 2025 has been released. 

-> RRB JE CBT 2 city intimation slip 2025 for June 4 exam has been released at the official website.

-> RRB JE CBT 2 Cancelled Shift Exam 2025 will be conducted on June 4, 2025 in offline mode. 

-> RRB JE CBT 2 Exam Analysis 2025 is Out, Candidates analysis their exam according to Shift 1 and 2 Questions and Answers.

-> The RRB JE Notification 2024 was released for 7951 vacancies for various posts of Junior Engineer, Depot Material Superintendent, Chemical & Metallurgical Assistant, Chemical Supervisor (Research) and Metallurgical Supervisor (Research). 

-> The selection process includes CBT 1, CBT 2, and Document Verification & Medical Test.

-> The candidates who will be selected will get an approximate salary range between Rs. 13,500 to Rs. 38,425.

-> Attempt RRB JE Free Current Affairs Mock Test here

-> Enhance your preparation with the RRB JE Previous Year Papers

Get Free Access Now
Hot Links: teen patti rich teen patti tiger teen patti master gold teen patti club apk